P-W-BRC-44 Effect of Pt or Gd Loaded ZSM-5 on Deactivation and Regeneration during JP-8 Cracking

Wednesday, June 5, 2013
Ballroom C (Galt House Hotel)
Sungtak Kim and Jochen Lauterbach, University of South Carolina, USA.
Pt and Gd are able to change catalytic activity and regenerability of ZSM-5 during JP-8 cracking. More importantly, not only the chemical structure of coke formation and carbon burn-off temperature but also the acid properties are significantly affected by the presence of Pt and Gd on ZSM-5.